Galvanic Corrosion
An accelerated form of corrosion occurring in an electrolyte when a pair of dissimilar metals capable of acting together as a source of electricity are in contact with each other. (New York City Economic Development Corporation, Waterfront Facilities Maintenance Management System, May 2016)